The Preventive Measures Of The Quality Problem Of Ribbon

- Jul 11, 2017 -

I. Curved Belt

Cause of formation:

1, steel buckle wear uneven 2, pan-head pulling yarn uneven 3, steel buckle position is not 4, the wrong way to pick up the yarn

Preventive measures:

1, the steel buckle wear method must according to the normal wear method, 1 group or 2 group wears the method. 2, the larger loose side, pull off some, until and the other side as flat or less 1-5 laps can be. 3, the steel buckle general and knitting needle distance, have a steel buckle empty distance can. 4, according to the needs of the ribbon, the upper and lower layer, or the points, the left and right, generally to be divided up and down, a belt if there are two or more practices or lines, it is necessary to separate.

II. UP wave

Cause of formation:

1, steel buckle wear yarn uneven, on both sides of the yarn too much, in the middle of wearing too little. 2, steel buckle wear too big, weft pull too tight. 3, the pan-head pulls the yarn uneven, pulls tightly on both sides, the middle pulls loose. 4, the yarn is not correct, the balance of falling pressure is not good.

Preventive measures:

1, the use of standard steel buckle, according to 1 or 2 groups of wear method. 2, according to the width of the ribbon needs, and then select the steel buckle to wear. 3, the middle and the two sides of the yarn to exchange a few, or the middle of the loose pull some down. 4, according to the Ribbon practice needs to be picked up, the balance of the number of the amount of pressure on average.